<p>In the state of-the art, Tungsten (W) as a crack prone material in laser processing is being investigated with different approaches that influence the cooling behavior and thermomechanical conditions during processing. Investigations in the present paper analyze the application of laser beam shaping and, therefore, the adjustment and homogenization of the laser intensity input at single weld lines on pure tungsten sheets. Additionally, the laser beam size in the processing zone is varied by a factor of max. 1.9. Experiments show that the reduction of the peak laser intensities, in the range of 9,120–9,600 kW/cm<sup>2</sup> at ring-shaped beam profiles, compared to laser intensities in the region of maximal 47,200 kW/cm<sup>2</sup> at Gaussian beam profiles result in a significant crack reduction and crack avoidance. Also contributing to the crack reduction is the emerging equiaxed solidification morphology in the fusion zone at applied ring-shaped beam profiles and at the enlargement of the Gaussian beam profile. Resulting lower laser intensities at larger beam profiles at a magnification factor of 1.9 at the ring-shaped beam profile and the Gaussian beam profile show, besides the crack avoidance, a high potential for a process speed enhancement at Powder Bed Fusion of Metals using a laser-based system (PBF-LB/M) in future applications. Therefore, concerning the melt pool geometry and the emerging microstructure, the Gaussian and ring-shaped beam profile at a comparable beam diameter show similar results. Due to the severe enlargement of the melt pool width at a decent penetration depth at aspect ratios d/w &lt; 0.5 in the conduction welding regime, adapted beam profiles can, therefore, drastically influence the cooling behavior with reduced cracking as well as enhance the process speed and eliminate process faults like keyhole porosity.</p>
Visa mer

Organisationer och upphovspersoner

Teknologiska forskningscentralen VTT Ab

Laukkanen Anssi Orcid -palvelun logo

Pinomaa Tatu Orcid -palvelun logo

Publikationstyp

Publikationsform

Artikel

Moderpublikationens typ

Tidning

Artikelstyp

En originalartikel

Målgrupp

Vetenskaplig

Kollegialt utvärderad

Kollegialt utvärderad

UKM:s publikationstyp

A1 Originalartikel i en vetenskaplig tidskrift

Publikationskanalens uppgifter

Volym

125

Artikelnummer

106864

Publikationsforum

58774

Publikationsforumsnivå

1

Öppen tillgång

Öppen tillgänglighet i förläggarens tjänst

Ja

Öppen tillgång till publikationskanalen

Delvis öppen publikationskanal

Licens för förläggarens version

CC BY

Parallellsparad

Nej

Övriga uppgifter

Vetenskapsområden

Maskin- och produktionsteknik; Materialteknik

Nyckelord

[object Object],[object Object],[object Object],[object Object],[object Object]

Identifierade tema

[object Object]

Språk

engelska

Internationell sampublikation

Ja

Sampublikation med ett företag

Nej

DOI

10.1016/j.ijrmhm.2024.106864

Publikationen ingår i undervisnings- och kulturministeriets datainsamling

Ja